配方类型: |
TEXTILES AND THEIR TREATMENT |
配方说明: |
Jet Dyeing Polyesters |
配方组成: |
(Residual Lubricants) The fabric should be clean and virtually free of lubricants (less than 0.25% on the goods) before dyeing. If prescouring is to be done in the jet machine, nonfoaming detergents such as "Tanapon" LCE, Tanapon NF or "Tanapon" INF should be used. (Air Leaks) The jet dyeing machine must be properly sealed and checked for air leaks. If not eliminated, leaks can cause foaming problems. (Dyes) High foaming disperse dyes should be avoided whenever p |
配制方法: |
(Prescour) When prescouring on the jet machine, use 1 g/l "Tanapon" NF or "Tanapon" LCE or "Tanapon" INF plus 1 g/l TSPP, soda ash or caustic soda. Run for 20 minutes at 140F. Rinse thoroughly with warm water. (Dyeing) Set dyebath cold (below 100F.) with "Tanavol" APJ. Run 5 minutes and add disperse dyes. Note: If high foaming dyes are used, add "Nofome" J or "Nofome" NS to suppress foam. Adjust pH to 4.5-5.0 with acetic acid. Raise temperature at 2-3F per minute to 250F and hold for 45 minutes to one hour. Adds, if needed, can be made at 180-190F. When on shade, cool slowly to 160-140F and overflow rinse until cool and clear. Dry and finish in the usual manner. |
|